Characteristics: 1. The slag deaeration ability, good separability, slag and molten copper slag loose and light, easy to steak is divided, and had no effect on the alloy composition and performance.
2. The economic benefit is obvious, the use of the solvents compared with these solvents are not applicable, can be more than the original 1% or so of the metal, and absolutely no stick wall, instead of borax, charcoal, and easy to moisture absorption used in the old process of sodium solvents.
Use scope: when this product is a kind of new energy and materials saving pollution-free copper refining slag removal agent, used for various grades of green, brass alloy, in smelting process in addition to gas, slag and covering effect, especially for the old material waste slag removal effect is more obvious.
Method of use: 1. To join the temperature of 900 degrees - 900 degrees, addition amount of copper liquid weight of 0.3% 0.6%.
2. Stay alloy melt completely, after solvent on liquid surface, stir well, stay with the copper liquid after full reaction, scum to the surface of copper liquid, then to wait out pouring.
Packaging storage: yellow powder 2 kg/bag, outer packing in cartons of 25 kg/box, the product shelf life for 18 months, beware of be affected with damp be affected with damp.